| Test equipment |
|
SIT_0005.jpg |
| Caption |
Test equipment for the determination of the susceptibility of metals to stress corrosion cracking |
|
| Size (Pixel): |
1770 x 1180 |
|
| Resolution: |
300 dpi |
|
| |
| |
| PVD equipment |
|
SIT_0014.jpg |
| Caption |
Physical vapour deposition (PVD) equipment for the development of customized functional coating systems |
|
| Size (Pixel): |
2048 x 1536 |
|
| Resolution: |
305 dpi |
|
| |
| |
| Pin-on-disk test rig |
|
SIT_0008.jpg |
| Caption |
Pin-on-disk test rig for the tribological qualification of mating materials and/or functional coatings |
|
| Size (Pixel): |
1770 x 1643 |
|
| Resolution: |
300 dpi |
|
| |
| |
| Atomic force Microscopy (AFM) |
|
SIT_0012.jpg |
| Caption |
Investigation of nanostructured surfaces at Sulzer Innotec using an atomic force microscope (AFM) |
|
| Size (Pixel): |
1770 x 1180 |
|
| Resolution: |
300 dpi |
|
| |
| |
| Starved lubrication experiments |
|
SIT_0009.jpg |
| Caption |
Pin-on-disk test setup for starved lubrication experiments and for the quantification of the performance of lubricants |
|
| Size (Pixel): |
3072 x 2048 |
|
| Resolution: |
300 dpi |
|
| |
| |